Hastelloy˘ B-3

This Nickel-Molybdenum alloy gives excellent resistance to hydrochloric acid at all concentrations and temperatures from ambient to high. It also withstands sulphuric, acetic, formic and phosphoric acids and other non oxidizing media. B-3 also has excellent resistance to pitting corrosion and to stress-corrosion cracking. Hastelloy B-3 is not recommended in the presence of ferric or cupric salts.

ASTM B335
ASTM B619
W.Nr 2.4600
UNS N10675
AWS 051
Excellent corrosion resistance to hydrochloric acid at all concentrations and temperatures
Withstands sulphuric, acetic, formic & phosphoric acids & other non-oxidising media
Excellent resistance to pitting corrosion & stress corrosion cracking
Chemical processing
Specifications
ASTM B335
ASTM B619
W.Nr 2.4600
UNS N10675
AWS 051
Excellent corrosion resistance to hydrochloric acid at all concentrations and temperatures
Withstands sulphuric, acetic, formic & phosphoric acids & other non-oxidising media
Excellent resistance to pitting corrosion & stress corrosion cracking
Chemical processing

Chemical Composition

Element Min % Max %
Ni 65.00
Cr 1.00 3.00
Mo 27.00 32.00
Fe 1.00 3.00
W 3.00
C 0.01
Si 0.10
Co 3.00
Mn 3.00
V 0.20
P 0.03
S 0.01
Ti 0.20
Cu 0.20
Al 0.50
Zr 0.10
Nb/Cb 0.20
Ta 0.20
Ni+Mo 94.00 98.00

Density

9.22 g/cm³ | 0.333 lb/in³

Melting Point

1418°C | 2585°F

Coefficient of Expansion

10.6 μm/m °C (20 – 100°C) | 5.7 x 10-6 in/in °F (70 – 212°F)

Modulus of Rigidity

83 kN/mm² | 12038 ksi

Modulus of Elasticity

216 kN/mm² | 31329 ksi

Heat Treatment of Finished Parts

Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed or Spring Temper Stress Relieve 400 – 450 750 – 840 2 Air

Properties

Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Annealed 1000 – 1200 145 – 174 -200 to +400 -330 to +750
Spring Temper 1600 – 2000 232 – 290 -200 to +400 -330 to +750
The above tensile strength ranges are typical. If you require different please ask.