Hastelloy˘ C-22

A Nickel-Chromium-Molybdenum alloy with better overall resistance and versatility than any other NiCrMo available. It has excellent resistance to localised corrosion and to a variety of mixed industrial chemicals.

Hastelloy C-22 is also known as Nicrofer 5621, Superimphy C22, and Inconel 622.

ASTM B574
ASTM B575
ASTM B619
ISO 15156-3 (NACE MR 0175)
W.Nr 2.4602
UNS N06022
AWS 053
Better overall corrosion resistance than Hastelloy C-4 & C-276 and Inconel 625
Outstanding resistance to pitting, crevice corrosion and stress corrosion cracking
Chlorination systems
Nuclear fuel reprocessing
Pickling systems
Specifications
ASTM B574
ASTM B575
ASTM B619
ISO 15156-3 (NACE MR 0175)
W.Nr 2.4602
UNS N06022
AWS 053
Better overall corrosion resistance than Hastelloy C-4 & C-276 and Inconel 625
Outstanding resistance to pitting, crevice corrosion and stress corrosion cracking
Chlorination systems
Nuclear fuel reprocessing
Pickling systems

Chemical Composition

Element Min % Max %
Cr 20.00 22.50
Mo 12.50 14.50
Fe 2.00 6.00
W 2.50 3.50
C 0.015
Si 0.08
Co 2.50
Mn 0.50
V 0.35
P 0.02
S 0.02
Ni Bal

Density

8.69 g/cm³ | 0.314 lb/in³

Melting Point

1399°C | 2550°F

Coefficient of Expansion

12.4 μm/m °C (20 – 100°C) | 6.9 x 10-6 in/in °F (70 – 212°F)

Modulus of Rigidity

78.6 kN/mm² | 11400 ksi

Modulus of Elasticity

205.5 kN/mm² | 29806 ksi

Heat Treatment of Finished Parts

Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed or Spring Temper Stress Relieve 400 – 450 750 – 840 2 Air

Properties

Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Annealed 800 – 1100 116 – 159 -200 to +400 -330 to +750
Spring Temper 1400 – 1700 203 – 247 -200 to +400 -330 to +750
The above tensile strength ranges are typical. If you require different please ask.