Hastelloy˘ C-276

This Nickel-Molybdenum-Chromium alloy with the addition of Tungsten, has excellent corrosion resistance in a wide range of corrosive media and is especially resistant to pitting and crevice corrosion.

Hastelloy C-276 is also known as Nicrofer 5716, Superimphy 276, and Inconel C-276.

ASTM B574
ASTM B575
ASTM B619
ISO 15156-3 (NACE MR 0175)
W.Nr 2.4819
UNS N10276
AWS 054
Excellent corrosion resistance in a wide range of corrosive media including, sulphur compounds and chloride ions
Excellent resistance to pitting, crevice corrosion and stress corrosion cracking
Withstands the corrosive effects of wet chlorine gas, hypochlorite and chlorine dioxide
Good for sea water applications.
Pollution control
Chemical processing
Waste treatment
Marine engineering
Pulp and paper production
Specifications
ASTM B574
ASTM B575
ASTM B619
ISO 15156-3 (NACE MR 0175)
W.Nr 2.4819
UNS N10276
AWS 054
Excellent corrosion resistance in a wide range of corrosive media including, sulphur compounds and chloride ions
Excellent resistance to pitting, crevice corrosion and stress corrosion cracking
Withstands the corrosive effects of wet chlorine gas, hypochlorite and chlorine dioxide
Good for sea water applications.
Pollution control
Chemical processing
Waste treatment
Marine engineering
Pulp and paper production

Chemical Composition

Element Min % Max %
Mo 15.00 17.00
Cr 14.50 16.50
Fe 4.00 7.00
W 3.00 4.50
Co 2.50
C 0.01
Si 0.08
Mn 1.00
V 0.35
P 0.04
S 0.03
Ni bal

Density

8.89 g/cm³ | 0.321 lb/in³

Melting Point

1370°C | 2500°F

Coefficient of Expansion

11.2 μm/m °C (20 – 100°C) | 6.2 x 10-6 in/in °F (70 – 212°F)

Modulus of Rigidity

78.6 kN/mm² | 11400 ksi

Modulus of Elasticity

205.5 kN/mm² | 29806 ksi

Heat Treatment of Finished Parts

Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed or Spring Temper Stress Relieve 400 – 450 750 – 840 2 Air

Properties

Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Annealed 850 – 1050 123 – 152 -200 to +400 -330 to +750
Spring Temper 1300 – 1700 189 – 247 -200 to +400 -330 to +750
The above tensile strength ranges are typical. If you require different please ask.