MP35N*

MP35N is an age hardenable Nickel-Cobalt base alloy that has a unique combination of properties – ultra high strength, toughness, ductility and outstanding corrosion resistance. MP35N resists corrosion in hydrogen sulphide, salt water and other chloride solutions. It also has excellent resistance to crevice and stress corrosion cracking in sea water and other hostile environments. Suitable where a high combination of strength, high modulus values and good corrosion resistance are required. Applications for this alloy also include medical devices and dental products.

MP35N is also known as Allvac 35N.

AMS 5844
AMS 5845
ASTM F562
ISO 15156-3
(NACE MR 0175)
ISO 5832-6
W. Nr. 2.4999
UNS R30035
AWS 110
Combination of high strength, ductility and good mechanical properties at ambient temperatures
Excellent corrosion resistance in hydrogen sulphide
Excellent resistance to crevice and stress corrosion cracking in sea water
Age hardenable (Spring Temper only)
Medical Devices
Marine Engineering
Specifications
AMS 5844
AMS 5845
ASTM F562
ISO 15156-3
(NACE MR 0175)
ISO 5832-6
W. Nr. 2.4999
UNS R30035
AWS 110
Combination of high strength, ductility and good mechanical properties at ambient temperatures
Excellent corrosion resistance in hydrogen sulphide
Excellent resistance to crevice and stress corrosion cracking in sea water
Age hardenable (Spring Temper only)
Medical Devices
Marine Engineering

Chemical Composition

Element Min % Max %
C 0.025
P 0.015
Si 0.15
Ni 33.00 37.00
Co bal
Mn 0.15
S 0.01
Cr 19.00 21.00
Mo 9.00 10.50
Ti 1.00
Fe 1.00

Density

8.43 g/cm³ | 0.304 lb/in³

Melting Point

1440°C | 1440°C

Coefficient of Expansion

12.8 μm/m °C (20 – 100°C) | 12.8 μm/m °C (20 – 100°C)

Modulus of Rigidity

80.7 kN/mm² | 11705 ksi

Modulus of Elasticity

234 kN/mm² | 33939 ksi

Heat Treatment of Finished Parts

Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed
Spring Temper Age Harden 650 1200 4 Air

Properties

Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Annealed < 1100 < 160 -200 to +315 -330 to +600
Spring Temper 1400 – 1900 203 – 276 -200 to +315 -330 to +600
Spring Temper + Aged 1900 – 2200 276 – 319 -200 to +315 -330 to +600
The above tensile strength ranges are typical. If you require different please ask.

*Trade name of SPS Technologies