Stainless Steel 316Ti

316 Ti is similar to 316L but has better high temperature strength and mechanical strength.

Stainless Steel 316Ti is also known as AISI 316Ti, Supra316Ti, Nirosta 4571, Polarit 761, and Remanit 4571.

ASTM A240
ISO 15156-3 (NACE MR0175)
BS EN 10088-3
W.NR 1.4571
UNS S31635
AWS 168
Better corrosion resistance at higher temperatures than 316 stainless.
Chemical processing.
Springs.
Fasteners.
Thread inserts.
Wire mesh.
Specifications
ASTM A240
ISO 15156-3 (NACE MR0175)
BS EN 10088-3
W.NR 1.4571
UNS S31635
AWS 168
Better corrosion resistance at higher temperatures than 316 stainless.
Chemical processing.
Springs.
Fasteners.
Thread inserts.
Wire mesh.

Chemical Composition

Element Min % Max %
C 0.08
Si 1.00
Mn 2.00
P 0.045
S 0.03
Cr 16.50 18.50
Mo 2.00 2.50
Ni 10.50 13.50
Ti 5 x C 0.70
Fe bal

Density

7.9 g/cm³ | 0.285 lb/in³

Melting Point

1375°C | 2500°F

Coefficient of Expansion

16.5 μm/m °C (21 – 100°C) | 9.110 x 10-6 in/in °F (70 – 212°F)

Modulus of Elasticity

193 kN/mm² | 27990 ksi

Modulus of Rigidity

74 kN/mm² | 10730 ksi

Heat Treatment of Finished Parts

Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed or Spring Temper Stress Relieve 250 480 1 Air

Properties

Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Annealed 600 – 750 87 – 109 -200 to +300 -330 to +570
Spring Temper 1300 – 1600 189 – 232 -200 to +300 -330 to +570
The above tensile strength ranges are typical. If you require different please ask.