Inconel® 600

A Nickel-Chromium alloy with good resistance to oxidation and corrosion at high temperatures.

Inconel® 600 is also known as Nicrofer 716, Pyromet Alloy 600, and Nicrimphy 600.

AMS 5665
AMS 5687
ASTM B166
BS 3075 NA 14
BS 3076 NA 14
DTD 328A
QQ-W-390
W.NR 2.4816
UNS N06600
AWS 010
Good Oxidation Resistance
Good Corrosion Resistance at High Temperatures
High temperature static applications**
Furnace Components
Chemical Processing
Food Processing
Nuclear Engineering
Specifications
AMS 5665
AMS 5687
ASTM B166
BS 3075 NA 14
BS 3076 NA 14
DTD 328A
QQ-W-390
W.NR 2.4816
UNS N06600
AWS 010
Good Oxidation Resistance
Good Corrosion Resistance at High Temperatures
High temperature static applications**
Furnace Components
Chemical Processing
Food Processing
Nuclear Engineering

Chemical Composition

Element Min % Max %
Ni 72.00
Cr 14.00 17.00
Fe 6.00 10.00
Mn 1.00
C 0.10
Cu 0.50
Si 0.50
S 0.015
P 0.04
Co 1.00
Nb/Cb 1.00
Ti 0.50
Ta 0.05
AI 0.35

Density

8.47g/cm³ | 0.306 lb/in³

Melting Point

1413°C | 2575°F

Coefficient of Expansion

13.3 μm/m | 7.4 x 10-6 in/in °F (70 – 212°F)

Modulus of Rigidity

75.6 kN/mm² | 10965 ksi

Modulus of Elasticity

206 kN/mm² | 29878 ksi

Heat Treatment of Finished Parts

Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed or Spring Temper Stress Relieve 460 860 1 Air

Properties

Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Annealed 600 – 850 87 – 123 -200 to +1000 -330 to +1830
Spring Temper 900 – 1450 131 – 210 -200 to +1000 -330 to +1830
Slight magnetisum may occur below 120°C (184°F)
The above tensile strength ranges are typical. If you require different please ask.
*Trade name of Special Metals Group of Companies
**Static application = Still/Fixed/Motionless/Rigid