Nitronic* 60

Nitronic 60 is an anti-galling and wear resistant stainless steel.

Nitronic 60 is also known as Alloy 218 and HPA 50.

AMS 5848
ASTM A580
UNS S21800
AWS 166
Anti galling
Wear resistant
Valve Stems
Pins
Brushes
Roller bearings
Pump shafts and rings
Thread inserts
Fasteners
Specifications
AMS 5848
ASTM A580
UNS S21800
AWS 166
Anti galling
Wear resistant
Valve Stems
Pins
Brushes
Roller bearings
Pump shafts and rings
Thread inserts
Fasteners

Chemical Composition

Element Min % Max %
C 0.10
Si 3.50 4.50
Mn 7.00 9.00
Ni 8.00 9.00
Cr 16.00 18.00
S 0.03
P 0.04
Mo 0.75
N 0.08 0.18
Cu 0.75
Fe bal

Density

7.6 g/cm³ | 0.28 lb/in³

Melting Point

1375°C | 2500°F

Coefficient of Expansion

15.8 μm/m °C (21 – 200°C) | 8.810 x 10-6 in/in °F (70 – 212°F)

Modulus of Elasticity

181 kN/mm² | 26200 ksi

Modulus of Rigidity

69 kN/mm² | 10008 ksi

Heat Treatment of Finished Parts

Condition as supplied by Alloy Wire Type Temperature Time (Hr) Cooling
°C °F
Annealed or Spring Temper Stress Relieve 250 480 1 Air

Properties

Condition Approx. tensile strength Approx. operating temperature
N/mm² ksi °C °F
Solution Annealed 700 – 1000 102 – 145 -200 to +300 -330 to +570
Spring Temper 1300 – 1900 189 – 276 -200 to +300 -330 to +570
The above tensile strength ranges are typical. If you require different please ask.